Ana amfani da shi a cikin Dental Metal Spherical Superalloy 3D Buga Foda Farashin CoCrW Foda

Takaitaccen Bayani:

Spherical Superalloy 3D Buga Foda Farashin CoCrW Foda


Cikakken Bayani

Tags samfurin

Bayanin Samfura

Spherical Superalloy 3D Buga Foda Farashin CoCrW Foda

CoCrW Foda Sunan samfur CoCrW Foda
Siffofin High Spherical, low oxygen abun ciki
Samfura masu dacewa UK Renishaw, GE EOS (EOSINT M jerin), Laser Concept, 3D tsarin
m dabara SLM/EBM, PM, Fesa
Yawowa ≤18s
Yawaita bayyananne ≥4.2g/cc
Oxygen abun ciki ≤200ppm
Nitrogen abun ciki ≤100ppm
karfin juyi 1100± 50Mpa
samar da ƙarfi 630± 50Mpa
girman barbashi 0 ~ 25μm,15-53μm, 45-105μm, 75-150μm
elongation 9± 2%
aikace-aikace 3D bugu foda, shafi

 

Takaddun shaida na CoCrW Foda (wt%)
Cr W Si Fe Mn Co
26.5-29 7.0-9.0 1.2 ~ 1.9 ≤0.6 ≤0.4 Ma'auni
Amfaninmu

Sabis za mu iya bayarwa

1) Ana iya sanya hannu kan kwangilar hukuma

2)Ana iya sanya hannu kan yarjejeniyar sirri
3) Garanti na dawowar kwana bakwai
Mafi mahimmanci: za mu iya samar da ba kawai samfurin ba, amma sabis na mafita na fasaha!

 

Shiryawa & Bayarwa

 

Don mafi kyawun tabbatar da amincin kayan ku, za a samar da ƙwararru, abokantaka na muhalli, dacewa da ingantaccen marufi.

 

Bayanin Kamfanin

Gabatarwar Kamfanin

Shanghai Epoch Material Co., Ltd yana cikin cibiyar tattalin arziki-Shanghai.Kullum muna bin “Kayan ci gaba, ingantacciyar rayuwa” da kwamitin bincike da haɓaka fasaha, don yin amfani da shi a rayuwar yau da kullun na ɗan adam don inganta rayuwarmu.

Yanzu, galibi muna ma'amala da kayan ƙasa marasa ƙarfi, kayan nano, kayan OLED, da sauran kayan haɓaka.Wadannan ci-gaba kayan ana amfani da ko'ina a cikin sunadarai, magani, ilmin halitta, OLED nuni, OLED haske, muhalli kare, sabon makamashi, da dai sauransu.

 

A halin yanzu, muna da masana'antar samarwa guda biyu a lardin Shandong.Yana da fadin kasa murabba'in mita 30,000, kuma yana da ma'aikata sama da mutane 100, wadanda mutum 10 daga cikinsu manyan injiniyoyi ne.Mun kafa layin samarwa da ya dace da bincike, gwajin gwaji, da samar da jama'a, sannan mun kafa dakunan gwaje-gwaje biyu, da cibiyar gwaji daya.Muna gwada kowane samfuri da yawa kafin bayarwa don tabbatar da samar da samfur mai inganci ga abokin cinikinmu.

 

Muna maraba da abokan ciniki daga ko'ina cikin duniya don ziyarci masana'antar mu da kafa kyakkyawar haɗin gwiwa tare!

Akwai wata tsohuwar magana a China cewa mun fi farin cikin ganin abokai da abokan ciniki daga ko'ina cikin duniya!

Kamfaninmu ya wuce ta tsarin gudanarwa na ISO 9001, kuma muna da namu tsarin SOP don samarwa, tallace-tallace, da bayan sabis na tallace-tallace!Da fatan za mu iya samar muku da kyakkyawan sabis na ƙwararru!

 

Tallan Talla

Maraba da duk abokan ciniki daga duk duniya!

Muna da abokan ciniki a duk duniya, kuma har yanzu, sun kafa kyakkyawar haɗin gwiwa tare da Sumsung, LG, LV, da sauran abokan ciniki da yawa, kuma don ƙarin bayani, da fatan za a tuntuɓe mu!

 

FAQ
1) Shin kuna sana'a ko kasuwanci?

Mu masana'anta ne, masana'antar mu tana cikin Shandong, amma kuma muna iya ba ku sabis tasha tasha ɗaya!
2) Sharuɗɗan biyan kuɗi:
T/T (canja wurin telex), Western Union, MoneyGram, Katin Kiredit, Tabbatar da Kasuwancin Alibaba, BTC (bitcoin), da dai sauransu.
3) Lokacin jagoranci
≤25kg: a cikin kwanaki uku na aiki bayan an biya biya.
> 25kg: mako guda
4) MisaliAkwai, za mu iya samar da ƙananan samfurori na kyauta don ƙimar ƙima mai kyau!

 

5) Kunshin

1kg a kowace jaka don samfurori,

25kg ko 50kg a kowace ganga, ko kamar yadda kuke buƙata.
6) Adana
Ajiye kwandon a rufe sosai a cikin busasshen wuri mai sanyi kuma mai cike da iska.

 